Nickel welding Wire, ErNiCu-7, Monel 400/K500 Welding Wire,
AWS A5.14 ErNiCu7, Monel 400/K500 Nickel Welding, nickel welding wire,
♦Welding Material Zita: Nickel welding Wire, ErNiCu-7, Monel 400/K500 Welding Wire
♦MOQ: 15kg
♦Fomu: MIG (15kgs/spool), TIG (5kgs/bhokisi)
♦Saizi: dhayamita 0.01mm-8.0mm
♦Saizi Yakajairwa: 0.8MM / 1.0MM / 1.2MM / 1.6MM / 2.4MM / 3.2MM / 3.8MM / 4.0MM / 5.0MM
♦Maitiro: Inopindirana neChitupa AWS A5.14 ASME SFA A5.14
Bata Isu Kuti Udzidze Zvakawanda!
ErNiCu-7 Yakavakirwa Material is Monel 400 uye Monel K500, Iyi welding wire inonyanya kushandiswa kugadzira MONEL400 alloy, MONELR404 alloy uye MOENLK-500 alloy ne tungsten inert-gasi welding, MGW uye yakanyura arc welding, uye inogona zvakare kushandiswa kugadzira pamusoro pesimbi. neMGW uye yakanyura arc welding.
Inokurudzirwa kushandisa Erni-1 nickel waya chivharo kune chaiwo gasi welding mamiriro.
ERNiCu-7 Chemical Composition
C | Al | Ni | Si | Mn | P | S | Fe | Cu | Ti | Zvimwe |
≤0.15 | ≤1.25 | 62.0-69.0 | ≤1.25 | ≤4.0 | ≤0.02 | ≤0.015 | ≤2.5 | Bal | 1.5-3.0 | ≤0.50 |
ERNiCu-7 Typical Welding Parameters
Diameter | Process | Volt | Amps | Shielding Gasi | |
In | mm | ||||
0.035 | 0.9 | GMAW | 26-29 | 150-190 | 75% Argon + 25% Helium |
0.045 | 1.2 | GMAW | 28-32 | 180-220 | 75% Argon + 25% Helium |
1/16 | 1.6 | GMAW | 29-33 | 200-250 | 75% Argon + 25% Helium |
0.035 | 0.9 | GTAW | 12-15 | 60-90 | 100% Argon |
0.045 | 1.2 | GTAW | 13-16 | 80-110 | 100% Argon |
1/16 | 1.6 | GTAW | 14-18 | 90-130 | 100% Argon |
3/32 | 2.4 | GTAW | 15-20 | 120-175 | 100% Argon |
1/8 | 3.2 | GTAW | 15-20 | 150-220 | 100% Argon |
3/32 | 2.4 | SAW | 28-30 | 275-350 | Yakakodzera flux ngaashandisei |
1/8 | 3.2 | SAW | 29-32 | 350-450 | Yakakodzera flux ngaashandisei |
5/32 | 4.0 | SAW | 30-33 | 400-550 | Yakakodzera flux ngaashandisei |
ERNiCu-7 Mechanical Properties
Condition | Tensile Simba MPa (ksi) | Yield Strength MPa (ksi) | Elongation% |
AWS reauirement | 480(70) Typical | Hazvina kutaurwa | Hazvina kutaurwa |
Yakajairika mhinduro sewelded | 530(77) | 360(53) | 34 |
•Hapana Preheat inodiwa, yakanyanya kupisa tembiricha 150 ℃ uye hapana PwHT inodiwa
•Zvishandiso zvakasiyana-siyana zvewelding zvinosanganisira kujoinha alloys kuNickel 200 uye copper-nickel alloys-.
•Inoshandiswa zvakanyanya mumashandisirwo emugungwa nekuda kwekupokana kwayo kune inoparadza mhedzisiro yemvura yegungwa nemvura ine brackish.
•Inogona kushandiswa MIG pamusoro pesimbi mushure mekutanga layer ine nickel 208
MOQ: 15kg
Fomu: MIG (15kgs/spool), TIG (5kgs/bhokisi)
Kukura: Diameter 0.01mm-8.0mmKukura Kwakafanana:0.8MM/1.0MM/1.2MM/1.6MM/2.4MM/3.2MM/3.8MM/4.0MM/5.0MM
Maitiro: Inopindirana neChitupa AWS A5.14 ASME SFA A5.14