Waspaloy, Waspaloy kunaya kwemvura inoomesa deformation superalloy

Product Detail

Waspaloy, Waspaloy kunaya kwemvura kuomesa deformation superalloy,
Waspaloy ndiro, Waspaloy mhete, Waspaloy tsvimbo,

Mazita Ekutengesa Anowanikwa: Waspaloy, GH4738, UNS N07001,W.Nr.2.4654.

Waspaloy is nickel base age inoomeswa superalloy ine yakanakisa tembiricha yesimba uye yakanaka corrosion resistance, kunyanya kune oxidation, pasevhisi tembiricha inosvika 1200 ° F (650 ° C) yekutenderera yakakosha maapplication, uye inosvika 1600 ° F (870 ° C. ) kune zvimwe, zvisinganyanyi kudiwa, maapplication.Iyo alloy's high-tembiricha simba inotorwa kubva kune yayo yakasimba mhinduro inosimbisa zvinhu, molybdenum, cobalt uye chromium, uye zera rayo rinoomesa zvinhu, aluminium uye titanium.Simba rayo uye kugadzikana mitsara yakakwira kupfuura iyo inowanikwa kune alloy 718.

 

Waspaloy Chemical Kuumbwa

C

S

P

Si

Mn

Ti

Ni

Co

Cr

Fe

Zr

Cu

B

Al

Mo

0.02 0.10

≤ 0.015

≤ 0.015

≤ 0.15

≤ 0.10

2.75 3.25

Bal

12.0 15.0

18.0 21.0

≤ 2.0

0.02 0.08

≤ 0.10

0.003 0.01

1.2 1.6

3.5 5.0

Waspaloy Physical Properties

Density (g/cm3 )

0.296

Kunyungudika (℃)

2425-2475

Emperature (℃)

204

537

648

760

871

982

Thermal kuwedzera coefficient
(mu/mu°F x 10E-6)

7.0

7.8

8.1

8.4

8.9

9.7

Thermal conductivity
(Btu • ft/ft2 • hr • °F)

7.3

10.4

11.6

12.7

13.9

-

Elastic modulus (MPax 10E3)

206

186

179

165

158

144

Waspaloy Alloy Typical Mechanical Properties

 

Condition

Tensile simba/MPa

Kushanda tembiricha

Solution annealing

800-1000

550ºC

Solution + kuchembera

1300-1500

Annealing

1300-1600

Chitubu chakapfava

1300-1500

¤(Iyo yakajairwa tembiricha yakadzikama kuita, bvunzo yepepa rekurapa kupisa)

Waspaloy Mitemo uye Zvinotsanangurwa

 

Bar/Rod/Wire/Forging Strip/Coil Sheet/Ndiro
ASTM B 637, ISO 9723, ISO 9724, SAE AMS 5704, SAE AMS 5706,
SAE AMS 5707, SAE AMS 5708, SAE AMS 5709, SAE AMS 5828,
SAE AMS 5544

Waspaloy Inowanikwa Zvigadzirwa muSekonic Metals

Inconel 718 bar, inconel 625 bar

Waspaloy Bars & Rods

Round bars/Flat bars/Hex bars, Saizi Kubva 8.0mm-320mm, Inoshandiswa kumabhaudhi, mabhaudhi uye zvimwe zvakasara

welding wire uye spring wire

Waspaloy Wire

Supply in welding wire uye spring wire mune coil fomu uye kucheka kureba.

Sheet & Plate

Waspaloy sheet & ndiro

Upamhi hunosvika 1500mm uye kureba kusvika 6000mm, Hukobvu kubva 0.1mm kusvika 100mm.

Kukurumidza & Zvimwe Kukodzera

Waspaloy Fasteners

Waspaloy zvinhu mumhando dzeBolts, screws, flanges uye zvimwe zvinomhanyisa, zvinoenderana nevatengi kutaurwa.

inconel strip,invar stirp,kovar stirp

Waspaloy strip & coil

Yakapfava mamiriro uye yakaoma mamiriro ane AB inopenya nzvimbo, yakafara kusvika 1000mm

Sei Waspaloy?

 Zera kuomesa nickel-based alloy, yakakwirira inoshanda simba mu1400-1600 ° F.Kuramba kwakanaka kune oxidation inoshandiswa mugasi turbine injini pa1400-1600 ° F mamiriro ekunze.Muna 1150-1150 ° F, Waspaloy inokambaira kuputika simba rakakwirira kupfuura mu718.

Pachiyero che 0-1350 ° F, simba rinopisa rinopisa kwenguva pfupi rakaipa kupfuura 718 alloy.

Waspaloy Application field:

Waspaloy inoshandiswa kuita gas turbine engine components zvinodaidzira simba rakawanda uye corrosion resistance at high operating temperatures uye missile systems.

 

Waspaloy is a precipitation-hardened deformed superalloy, kushanda tembiricha haipfuure 815 ℃. The alloy ine goho guru simba uye kuneta kuramba pa 760 ℃ ~ 870 ℃, uye yakakwirira oxidation uye ngura kuramba pa 870 ℃, iyo yakakodzera kugadzira WO discs. , mashizha ekushanda, zvigadziro zvekushisa zvakanyanya, zvivharo zvemoto, shafts uye WO turbine kesi.Zvigadzirwa zvikuru zvinotonhora zvakaputirwa tambo uye inopisa inopisa pepa, pombi, tambo, tambo, forgings uye bolt fasteners, nezvimwewo.
Chimiro chinoenderana: W.nr 2.4654, UNS N07001, AWS 170
Inoshanda chiyero: AMS 5544 AMS 5708 AMS 5828